Thermally toughened safety glass conforming to BS EN 12150-1, subjected to secondary Heat Soak Testing (HST to BS EN 14179) to eliminate spontaneous nickel sulphide (NiS) inclusions.
SEND PROJECT DETAILS →| Standard | BS EN 12150-1 & BS EN 14179-1 (Heat Soak Tested) |
|---|
| Fracture Pattern | Shatters into small blunt granular fragments (< 1 cm²) without sharp shards |
|---|
| Bending Strength | 120 N/mm² surface compression stress (vs 45 N/mm² annealed float) |
|---|---|
| Thermal Shock Resistance | Withstands temperature differentials up to 200°C |
Manufactured in Türkiye under European BS EN quality regimes. Full traceability with third-party lab testing and mill certificates supplied with every bill of lading.
Submit your architectural project bill of quantities (BOQ), tender drawings, or required schedule. Our technical team returns guaranteed DDP / FOB factory pricing and testing certifications within 24 hours.